当前位置:主页 > 产品资料 >

橡胶气囊加工工艺


    橡胶气囊加工工艺:
   
Rubber air bag processing technology:
  <a href='/' target='_blank'><u>橡胶气囊</u></a>加工工艺:
   1、橡胶出产模型制品的去边修整,使制品表面光洁、外形尺寸达到要求;
   
1. Trimming of rubber production model products to make the surface of products bright and clean and the external dimensions meet the requirements;
   2、 通过一些特殊工艺加工,如对制品表面进行处置,使特殊的一种用途的制品的运用性能有所提髙;
   
2, through some special processing, such as the treatment of the surface of the products, so as to improve the performance of a special purpose of the products;
   3、对含有织物骨架的制品如胶带、轮胎等制品要进行热拉伸冷却和硫化后在充大气的压力力下冷却,以担保制品尺寸、形状牢稳和令称呼心的运用性能。
   
3, the fabric containing the framework of products such as rubber tape, tires and other products to hot stretch cooling and curing in the air under the pressure of cooling, to ensure that the size of the products, shape is stable and make the heart of the application of performance.
橡胶<a href='http://www.chinakqth.com/' target='_blank'><u>空气弹簧</u></a>
   橡胶出产模型在硫化时,胶料毕然会延着出产模型的分型面等部位流出,形成溢流胶边,也称为毛边或飞边,胶边的多少及厚薄决定于出产模型的结构、精确度、平板硫化机平板的平行度和装胶余胶量。现在的没有边际出产模型出产的制品,胶边尤其薄, 有时刻起模时就被带掉或轻轻一擦就可以去掉。但这种出产模型成本较高,易损伤,大部分数橡胶模制品在硫化在这以后都需求修整处置。
   
During vulcanization of rubber production model, the rubber material will flow out along the parting surface and other parts of the production model, forming an overflow rubber edge, also known as rough or flying edge. The amount and thickness of the rubber edge is determined by the structure, precision of the production model, the parallelism of the plate vulcanizing machine and the amount of glue left after loading.Now there is no marginal production model products, plastic edge is particularly thin, when there is a moment from the mold is taken away or gently wipe can be removed.But this production model cost is high, easy to damage, most of the rubber mold products in vulcanization after this need to repair disposal.
上海松夏橡胶接头